Re: [MW:30778] Unequal wall thickness in piping

1,760 views
Skip to first unread message
Message has been deleted

Dinesh Somwanshi

unread,
Apr 16, 2020, 11:30:23 PM4/16/20
to materials-welding
It's shall not lowered down to design thicknesses.

You may do smooth  tempering to match if above meets.

Dinesh

On Thu, Apr 16, 2020, 19:31 QA/QC <adnan...@gmail.com> wrote:
Hello everyone 

im asking for any information about the maximal thickness to weld between two different wall thickness  from  B31.3 or b.16.25 

in my case we want to weld  12'' THICKNESS 25.4 WITH 12.7 ITS POSSIBLE RE-SCHDULING THE INTERNAL THICKNESS FOR 12MM OR THER IS A MAXIMUM THICKNESS LIMITS 

BEST REGARDS

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f4e88916-9f58-4f94-8cad-5d6e69c079dc%40googlegroups.com.

atul khatri

unread,
Apr 17, 2020, 2:32:36 AM4/17/20
to material...@googlegroups.com
you can weld two dissimilar thick pipes and fittings by making proper transition of higher thickness to lower thickness.
Transition slope should be 1:3. Please refer figure UW-13.1 of ASME VIII DIV 1 for better understanding.

Best regards
Atul Khatri


Message has been deleted

james gerald

unread,
Apr 17, 2020, 6:56:27 AM4/17/20
to material...@googlegroups.com
Please find snap shot of ASMEB 31.3 below.

Inline image


ID Alignment may be done as per below sketch



Inline image

OD variation in Thickness may be Tapered to a slope of 1:3 (thickness : Length)


Thanks & Regards

J.Gerald Jayakumar




On Friday, April 17, 2020, 05:13:56 PM GMT+7, Adnan Ziad <adnan...@gmail.com> wrote:


more explaination please if you can 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

George Dilintas

unread,
May 9, 2020, 11:31:55 PM5/9/20
to material...@googlegroups.com
Read QW-202.4 in ASME IX