AISI 4130 MATERIALS

626 views
Skip to first unread message

bhaskar rao

unread,
May 30, 2011, 8:19:24 AM5/30/11
to material...@googlegroups.com
Dear Experts,
 
Please give me the answer regarding P No.
 
What is P No. of   AISI-4130 Material.
 
Thankyou & Best Regards,
 
 
PBRAO.

Harish Kannepalli

unread,
May 30, 2011, 12:49:53 PM5/30/11
to material...@googlegroups.com
asme equivalent p.no is 4 comes in 1 Cr- 0.5 Mo steels. like sa387 gr11

2011/5/30 bhaskar rao <pbra...@gmail.com>
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

K.Babu

unread,
May 31, 2011, 6:02:41 AM5/31/11
to material...@googlegroups.com
Unlisted


 
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu

Vincent

unread,
Jun 12, 2011, 2:21:47 AM6/12/11
to material...@googlegroups.com
the P No. is 11b, You can get it form AWS codes.

2011/5/31 K.Babu <kbab...@gmail.com>

vipin george

unread,
Jun 12, 2011, 12:33:08 PM6/12/11
to material...@googlegroups.com
Hi!
AISI 4130 is an unlisted material as per ASME .