Dear all Experts,


We are trying  to weld Ti to Ti & Ti to MS With GTAW Process ERTi-2 wire , can any one suggest the WPS for the same



Ti to Ti

Ti to MS

 

Base metal Grade (P no & Grp No)

P 51 to P51 

P 51 to P51 

Group No 51.2, UNS R50400

Thickness of the BM

8mm

8mm

 

Joint type

Butt weld

Butt weld

 


 



Thanks & Regards,