WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?

meisam shokri arfaei

unread,
Apr 23, 2015, 11:54:25 AM4/23/15
to material...@googlegroups.com
Charpy test is type of test to measure the resistance of a material to shock type stresses whether in room or minus temperatures. 

CTOD (Crack Tip Opening Displacement) is for measuring the resistance of material to cyclic type of stresses whether in room or minus temperatures.

So the main difference is the type of load which used during the test. So the specimens preparation and test procedures are different.

Regards

On Thu, Apr 23, 2015 at 12:42 PM, S.Mohammed <mohd...@gmail.com> wrote:
DEAR ALL

WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9c17d172-8437-41a1-a1bd-4cfe563a9350%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





Rajaram chandrasekaran

unread,
Apr 23, 2015, 11:54:59 AM4/23/15
to material...@googlegroups.com
dear friend

charphy test is evaluating the impact value(observed energy) by breaking the Specimen.
The speciment is from the material to be tested, and the specimen will have a "V"notch.


the CTOD test specimen will have the measured crack ,and will give the impact energy ,based on the development of crack extension, the impact energy will be decided.

thanks and regards
rajaram.c 

On Thu, Apr 23, 2015 at 12:12 PM, S.Mohammed <mohd...@gmail.com> wrote:
DEAR ALL

WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?

mohd firdaus

unread,
Apr 23, 2015, 11:55:35 AM4/23/15
to material...@googlegroups.com
Charpy V Notch are acceptance method for assessing resistance to brittle fracture. Usually use for develop WPS, material and consumable confirmation. CTOD measures a material property which is fracture toughness. Usually CTOD are use to measured in-service equipment. This is for estimation lifetime of equipment/material that load under certain stress condition and temperature.

Mohd Firdaus Abd Rahim
QA/QC
+60122796361

Sent from my iPhone

> On 23 Apr 2015, at 4:12 PTG, S.Mohammed <mohd...@gmail.com> wrote:
>
> DEAR ALL
>
> WHAT IS DIFF BETWEN CHARPY TEST AND CTOD TESTING?
>

Jim Price

unread,
Apr 23, 2015, 11:55:42 AM4/23/15
to material...@googlegroups.com

Alan Denney

unread,
Apr 24, 2015, 10:28:49 AM4/24/15
to material...@googlegroups.com

The reply below is incorrect: CTOD is not related to cyclic stresses. Both Charpy and CTOD measure fracture toughness. However Charpy is empirical whereas CTOD is a method of measuring material toughness such that the results can be used in fracture mechanics calculations to determine the criticality of material flaws of a known size in that material and corresponding microstructure. CTOD has its notch sharpened by fatigue cracking, but that is to give a very start initiator for the test only. The specimen should be the full thickness of the component to which the test relates, and the test temperature should be the minimum design temperature.

 

CTOD testing is inherently more complex and is much more expensive that Charpy testing and requires laboratories which are rather more specialised than those which can perform Charpy.

 

Alan Denney

meisam shokri arfaei

unread,
Apr 24, 2015, 12:29:37 PM4/24/15
to material...@googlegroups.com
Dear Alan,

I think there is a misunderstanding about my reply. I didn't say that the test is based on cyclically loading of the specimen. 

Also this is true that the mechanism of inducing the crack is by fatigue loading type and this will continued by the three point bending for studying the behavior of the material under loading. 

But after the test we use the results to calculate the critical defect/crack size and in most cases this parameter uses in cyclically loading conditions (this was my viewpoint). 

Also the results may use in FFS evaluations or it may use just for characterization of a material (whether metallic or non-metallic).

Regards


For more options, visit https://groups.google.com/d/optout.

Alan Denney

unread,
Apr 25, 2015, 12:30:50 AM4/25/15
to material...@googlegroups.com

I fully understand, Meisam. The results of the test are used in fracture mechanics analysis to determine the critical defect size for fracture. If the service loading includes cyclic stresses then these are taken into account in that analysis. The defect has to be ‘grown’ using the ‘Paris law’ and that grown defect has to be less than that critical defect size for fracture.

 