ASME Section 9

109 views
Skip to first unread message

Kannayeram Gnanapandithan

unread,
Jul 16, 2016, 9:12:43 AM7/16/16
to materials-welding
Having 2 PQRs ,one with PWHT and another without PWHT. With these 2 PQRS, can a single WPS be made addressing both conditions by keeping other variable in the order..

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

p_cha...@mail.bg

unread,
Jul 18, 2016, 9:11:41 PM7/18/16
to material...@googlegroups.com

Yes, you can, as long as all other variables are equal. 

Best regards

Dr. Parvan Chavdarov

----- Цитат от Kannayeram Gnanapandithan (kgpan...@gmail.com), на 15.07.2016 в 06:13 -----

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO%3DEaB2TgXQB8Usw52QYPOdFDvP_9ZrGPkUJNLKSdL%3DLQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



-------------------------------------
Mail.BG: Безплатен e-mail адрес. Най-добрите характеристики на българския пазар - 30 GB пощенска кутия, 1 GB прикрепен файл, безплатен POP3, мобилна версия и други.

Dinesh Gaur

unread,
Jul 19, 2016, 9:41:34 AM7/19/16
to material...@googlegroups.com
Dear Mr.Parvan
             Can you brief that on what basis you can made a single WPS?

As per ASME Sec IX, You Can"t.


pgoswami

unread,
Jul 19, 2016, 9:57:57 AM7/19/16
to material...@googlegroups.com, kgpan...@gmail.com

Mr. Pandithan,

 

PWHT is an essential variable for any welding procedure. Hence incorporating 2 PQR’s in one WPS with PWHT & No-PWHT could be confusing. Advice would be to make 2 separate Welding Procedures referencing 2 separate PQR’s . Please look under QW-407 for explanations.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 


--

John Henning

unread,
Jul 19, 2016, 11:00:32 AM7/19/16
to material...@googlegroups.com

Yes you can.

 

Section IX does not dictate the form of the WPS (or the PQR for that matter) but only dictates the variables or components that must be addressed.  A single WPS can be written for both conditions as long as the essential variables and non-essential variables are addressed for both conditions (and if appropriate, supplementary essential variables).   I have frequently seen WPS’s of this type and upon review have approved them on the basis of addressing all required variables.   In a previous job, it was not uncommon to weld a single coupon, split it into two parts and test one half with PWHT and the other tested as welded and then write a single WPS.  However, a single welded coupon is not required. 

 

The biggest problem is to avoid confusion for the welder caused by a too complex a WPS.  Remember that the ultimate purpose of the WPS is to provide guidance to the welder on how to complete the weld. 

 

Don’t import your personal bias into requirements for qualification.  Apply what is required by the Code and, if necessary, the ever annoying customer.

 

Enjoy. 

Kannayeram Gnanapandithan

unread,
Jul 19, 2016, 12:12:02 PM7/19/16
to materials-welding

PWHT is not essential for Welder and He need not bother about PWHT. Confusion will come in recording variable and preplanning is very much essential for each joint

Reply all
Reply to author
Forward
0 new messages