What Will be a F Number of E 2209-16 Welding rod (SMAW ).

311 views
Skip to first unread message

P NAVEEN

unread,
Mar 13, 2024, 7:15:06 AM3/13/24
to Materials & Welding
Dear Sir's,

I am Planning to weld the SS2205 to SS 2205 material .   

Which filler rod ( SMAW ) we can use on that , If we can use the E 2209-16, What will be a F Number of that.

Thanks 

Madhava Ram

unread,
Mar 13, 2024, 8:25:27 AM3/13/24
to material...@googlegroups.com
Consider F-05
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8f61ea7b-e1bc-4b4a-b6f6-25601536267en%40googlegroups.com.


--
With Regards,


Madhavaram E

Yutian Ren

unread,
Mar 14, 2024, 3:32:20 AM3/14/24
to material...@googlegroups.com
It can be E2209-16. 

P NAVEEN <pnave...@gmail.com> 于2024年3月13日周三 19:14写道:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Prathab P

unread,
Mar 14, 2024, 10:01:42 PM3/14/24
to material...@googlegroups.com

Azmy Ashoush

unread,
Mar 14, 2024, 11:55:29 PM3/14/24
to material...@googlegroups.com
Hi

F-No. For SFA A5.4 E2209-16 as per table QW-432 is 4

Thanks 


P NAVEEN

unread,
Mar 15, 2024, 3:08:55 AM3/15/24
to Materials & Welding
Sir, Why Not This one F No :- 5.
QW 432.pdf

p NAVEEN

unread,
Mar 15, 2024, 3:08:56 AM3/15/24
to material...@googlegroups.com
  1. 5 SFA-5.4 austenitic and duplex EXXX(X)-16 ... Why not this one. 

QW 432.pdf

Azmy Ashoush

unread,
Mar 15, 2024, 6:05:10 AM3/15/24
to material...@googlegroups.com

Hi 
I mean F-No. 5 not 4. 4 just typo
Thanks,
Best Regards 

 AZMY ASHOUSH

Head Of Marine Welding Section / IWE, CSWIP

PETROJET Marine 

Mobile: 01064908985

E-Mail: azmya...@petrojet.com.eg

              marinewe...@gmail.com


JIJILAL K M

unread,
Mar 21, 2024, 3:08:16 AM3/21/24
to material...@googlegroups.com
Dear Naveen,

ASTM A 790 ((UNS S32205) is a Ferritic/Austenitic SS Pipe having Cr.22-23% and Ni 4.5 - 6.5 %. which has P No. 10 H.
For welding this material using SMAW method , AWS SFA 5.4 E-2209 -16 is well suited which has F No.5.

Warm Regards,
Jiji Lal K M
CSWIP 3.1,ASNT LII,IRCA LA
QA/QC Manager,DHPL Pipeline Project
Corrtech International Limited.







--