Dear All,
 
pl.guide me anybody, wether the wps for tky jonts in pipe as per BS EN 15614 is qualified  for all type of joints in pipe and plate or not?
--
Thanks & Regards,

SHANMUGA GANESH B.E, D.M.E.M.,
Certified Welding Inspector-AWS
ASNT Level II (RT, UT, MT, PT, VT)
Inspection Engineer.
ABC Technical Consultancy
Sharjah,UAE.
Ph No: +971 55 975 4801

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Sudhakar

unread,
Apr 16, 2010, 10:21:25 PM4/16/10
to material...@googlegroups.com, material...@googlegroups.com
Dear Shanmugam,
The wps which is qualified for tky as per ISO 15614-1 qualifies for tky joints only in both plate and pipe.  
The dia limitations, thickness and the branch angle are essential variables.

Sent from my iPhone


Rgds
K.Sudhakar