what is pre qualified WPS as per AWS D1.1

2,478 views
Skip to first unread message

Anil Kumar

unread,
Nov 13, 2016, 8:30:56 AM11/13/16
to Materials & Welding
Other recipients:
Dear All What is pre qualified WPS as per AWS D1.1 Its allows to write a WPS without PQR...? Please explain Regards Samshuddin.K
Dear All

What is pre qualified WPS as per AWS D1.1

Its allows to write a WPS without PQR...?

Please explain

Ahmad el-sharkawy

unread,
Nov 13, 2016, 9:21:11 PM11/13/16
to material...@googlegroups.com

Yes allow use to write WPS withoutsupporting PQR.

--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ab0e459-ae40-446f-9f89-771c317b39e4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

pankaj phuse

unread,
Nov 14, 2016, 12:36:39 AM11/14/16
to Materials & Welding
Prequalified welding procedure specification includes a weld joint specified in a governing code that does not require validation of welding parameters through the performance of a procedure qualification test. So, a prequalified WPS does not need a supporting Procedure Qualification test Record (PQR).

Regards
Pankaj Phuse
Welding Engineer
CSWIP 3.1

c sridhar

unread,
Nov 14, 2016, 10:39:41 PM11/14/16
to material...@googlegroups.com
It means if you have already qualified a procedure for similar P nos, 
say, as per ASME sec IX  or any code, you can refer it in your new 
WPS if done with AWS D 1.1 for same P nos. No need to do a PQR 
for the new WPS.

Sridhar.



From: pankaj phuse <pankaj...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Monday, 14 November 2016 10:41 AM
Subject: [MW:25687] Re: what is pre qualified WPS as per AWS D1.1

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/035b3dca-c195-40db-b4e4-ac04f2d0e618%40googlegroups.com.

pankaj phuse

unread,
Nov 15, 2016, 2:48:38 AM11/15/16
to Materials & Welding, sridh...@yahoo.com
Dear Sridhar,

Here we are talking about Pre-Qualified WPS i.e..pWPS.
To initiate the welding, pWPS required.

Mhaskar Aly

unread,
Nov 26, 2016, 9:48:49 PM11/26/16
to material...@googlegroups.com, c sridhar

Prequalfied  wps means you can use welding processes, base metal, filler metal and other welding variables as given in AWS D1.1 only..you can't deviate  otherwise you need to qualify it.

Hope to have your understanding on above
Aly


To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5827c8e3-c316-40d2-a967-4a55eeef7cf5%40googlegroups.com.

VERD

unread,
Dec 13, 2019, 12:16:22 AM12/13/19
to Materials & Welding
What about the WPQ?


On Sunday, November 13, 2016 at 8:21:11 PM UTC-6, ahmad elsharkawy wrote:

Yes allow use to write WPS withoutsupporting PQR.

--

WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.

On Nov 13, 2016 3:30 PM, "Anil Kumar" <anilmo...@gmail.com> wrote:
Other recipients:
Dear All What is pre qualified WPS as per AWS D1.1 Its allows to write a WPS without PQR...? Please explain Regards Samshuddin.K
Dear All

What is pre qualified WPS as per AWS D1.1

Its allows to write a WPS without PQR...?

Please explain

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages