( P NO.1 G 2 ) to ( P NO 1 G 2 or 1 " ASTM A 519 )
Use ER 70S-6 or -3 // 100% co2 // PWHT & preheat according to thickness "check ur construction code "
Ahmed Osman
Welding Eng.
ASNT NDT level III
API 510 inspector
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMWFVQTb-3dpUmQjJ4NhHjK2oJz0scYop8Ef942i00qFLA%40mail.gmail.com.