dissimilar thickness welding

108 views
Skip to first unread message

shaik amjad

unread,
Nov 19, 2016, 2:16:01 AM11/19/16
to Materials & Welding
i need to prepare a WPS for plate 355j2 and S355JR thickness 5 mm. but i cant find 5mm plate for 355j2 grade. so can go for dissimilar thickness as 5mm S35Jr and 6mm S355J2 then what would be the thickness qualified range and impact testing requirement.

George Dilintas

unread,
Nov 20, 2016, 9:23:56 PM11/20/16
to Meghanadh K
according to which standard? ASME IX or EN 15614-1?
Assuming ASME IX and Pno 1 (I cant remember if 355J2 and 355JRis listed in ASMEIX)
with 5 mm to 6mm in PQR, the WPS ranges will be:
Thickness of thinner member : 1,5 to 10 mm
Thickness of thicker member 1,5 to 12 mm
In case when impact test is required:
the minimum for the thicker member will be 3 mm and for the thinner 2,5 mm.
In case of En 15614-1, no provision for dissimilar thickness 

2016-11-19 9:07 GMT+02:00 shaik amjad <amjadsh...@gmail.com>:
i need to prepare a WPS for plate 355j2 and S355JR thickness 5 mm. but i cant find 5mm plate for 355j2 grade. so can go for dissimilar thickness as 5mm S35Jr and 6mm S355J2 then what would be the thickness qualified range and impact testing requirement.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7a7a3ca7-62a8-42ad-8998-ac321a27c7dd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

shaik amjad

unread,
Nov 22, 2016, 6:50:46 AM11/22/16
to Materials & Welding
Dear Sir

Thanks a lot for the reply .... the code is AWS D1.1 , can i prepare wps for this dissimilar thickness(6mm to 5mm ) as per AWS D1.1

On Monday, 21 November 2016 06:23:56 UTC+4, George Dilintas wrote:
according to which standard? ASME IX or EN 15614-1?
Assuming ASME IX and Pno 1 (I cant remember if 355J2 and 355JRis listed in ASMEIX)
with 5 mm to 6mm in PQR, the WPS ranges will be:
Thickness of thinner member : 1,5 to 10 mm
Thickness of thicker member 1,5 to 12 mm
In case when impact test is required:
the minimum for the thicker member will be 3 mm and for the thinner 2,5 mm.
In case of En 15614-1, no provision for dissimilar thickness 
2016-11-19 9:07 GMT+02:00 shaik amjad <amjadsh...@gmail.com>:
i need to prepare a WPS for plate 355j2 and S355JR thickness 5 mm. but i cant find 5mm plate for 355j2 grade. so can go for dissimilar thickness as 5mm S35Jr and 6mm S355J2 then what would be the thickness qualified range and impact testing requirement.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages