Acceptance criteria for storage tanks

528 views
Skip to first unread message

Kareem Sheikh

unread,
Aug 8, 2018, 8:12:03 AM8/8/18
to material...@googlegroups.com
Good day,

Please share acceptance criteria of UT & DPE for storage tanks.

Your prompt response in this regards will be highly appreciated.

Hasin Shaikh

unread,
Aug 8, 2018, 8:57:30 AM8/8/18
to material...@googlegroups.com
Dear Kareem

For UT it has mentioned in API 650 Clause 8.3.2.5 & for DPE  Clause 8.4.4

8.3.2.5 says acceptance standard shall be agreed upon by the Purchaser and the Manufacturer

8.4.4 says acceptance standard and removal and repair of defect shall be in accordance with Section VIII,Annex 8,Para 8-3,8-4 and 8-5 of ASME Code.

With Regards
Hasin Shaikh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
*With Regards
Shaikh.Hasin
Email: hasin....@gmail.com
Mobile: +91-9924562942*


Reply all
Reply to author
Forward
0 new messages