http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n-WNLDxx1b6%3Daqu_my_rTKo8HKme9cWQsamH5NKVJMbQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
| From: Kannayeram Gnanapandithan Sent: Τετάρτη, 31 Αυγούστου 2016 - 08:38 To: materials-welding Reply To: material...@googlegroups.com Subject: Re: [MW:25334] Hardness Value For the P-91 and SS material. |
|
From: Kannayeram Gnanapandithan
Sent: Τετάρτη, 31 Αυγούστου 2016 - 08:38
To: materials-welding
Reply To: material...@googlegroups.com
Subject: Re: [MW:25334] Hardness Value For the P-91 and SS material. |
Dear Everybody,How much is Lower & Upper hardness limit with code reference for the weldment of ASTM-A-335 Gr. P-91 To A312 TP 316 with filler combination ER-Ni Cr3.Regards,Pradip
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n-WNLDxx1b6%3Daqu_my_rTKo8HKme9cWQsamH5NKVJMbQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Don't weld P91 directly to Stainless steel,
Embrittlement off one or both of the materials will be your part, depending on the PWHT.This is a serious warningJPrinsen MSc, IWE
Van: dili...@gmail.com
Aan: "Kannayeram Gnanapandithan" <materials-welding@googlegroups.com>, "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 1 september 2016 15:42:00
Onderwerp: Re: [MW:25339] Hardness Value For the P-91 and SS material.
According to the bibliography min hardness on P91 should be 191 HVSent from my BlackBerry 10 smartphone.
From: Kannayeram GnanapandithanSent: Τετάρτη, 31 Αυγούστου 2016 - 08:38To: materials-welding
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:25334] Hardness Value For the P-91 and SS material.
Hardness only on HAZ of P91 is to be around 230Hv
THANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITYMobile no: +919940739349
On Tue, Aug 30, 2016 at 9:59 AM, pradip kumar Sil <prad...@gmail.com> wrote:
Dear Everybody,How much is Lower & Upper hardness limit with code reference for the weldment of ASTM-A-335 Gr. P-91 To A312 TP 316 with filler combination ER-Ni Cr3.Regards,Pradip
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n-WNLDxx1b6%3Daqu_my_rTKo8HKme9cWQsamH5NKVJMbQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNaPwK%3DOZMxuh0ZPWExJGYeu7qY%3D7thZ6JkX7X2oCVNiQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160901134200.6713430.77205.4290%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/17328743.23160343.1472739238467.JavaMail.zimbra%40online.nl.