PWHT of blind flanges

46 views
Skip to first unread message

Muhammed Ibrahim PK

unread,
Sep 4, 2025, 9:06:54 AMSep 4
to material...@googlegroups.com
Dear All,

Is it required to place permanent blind flanges in the furnace when the vessel requires PWHT ?. 

If there is handle welded on blind flange, PWHT required ?


Thanks & Regards
Muhammed Ibrahim PK

sridhar cn

unread,
Sep 4, 2025, 11:43:09 AMSep 4
to material...@googlegroups.com
Permanent blind flanges may not require PWHT, any welds associated with them typically do, if they affect 
the structural integrity. But if the handle is a temporary weldment, and removed later or if the fillet is small,
then PWHT is not needed. 
C Sridhar.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALOPgmMeBUXfY3uqO9JdxG3cSLXtEVvrnekekCZFs%2BBV%2BDOAmw%40mail.gmail.com.

Mohd Siraj

unread,
Oct 23, 2025, 11:08:41 AMOct 23
to Materials & Welding
which type of gasket u will use to fix permeant blind flange?

venkateswara reddy Desireddy

unread,
Oct 23, 2025, 12:05:36 PMOct 23
to material...@googlegroups.com
Blind Flanges (manhole or other) are keep separate in farnace. Don't assemble with vessel. 

Flanges serrations need to protect, apply chalk powder .

Welded flanges will do PWHT along with vessel. Because of flanges thickness.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages