Qualification of welders

78 views
Skip to first unread message

mervin dio

unread,
Oct 20, 2015, 11:49:13 PM10/20/15
to material...@googlegroups.com
Dear members


I have some question about the welders qualification because in our project the welders is qualified to carbon steel materials. He can weld to higher P-No like P4. As per asme QW 423.1 he is qualifiy to weld. Pno is essential variables to Welders. Can you please give me some information about this.


Regards

Kannayeram Gnanapandithan

unread,
Oct 21, 2015, 11:41:14 PM10/21/15
to materials-welding
provided all other essential variable are taken care

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1445393918.82603.YahooMailAndroidMobile%40web181503.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

raouf salhi

unread,
Oct 22, 2015, 5:01:20 AM10/22/15
to material...@googlegroups.com
Dear Mervin ,

yes P number is essential variable for welder's qualification.

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258



JIJILAL K M

unread,
Oct 22, 2015, 5:16:46 AM10/22/15
to material...@googlegroups.com
Dear Mervin,

ASME P1 qualified welders can weld ASME P4 without further welder test.

K M Jijilal




K.M. JIJILAL


--

c sridhar

unread,
Oct 24, 2015, 1:17:38 AM10/24/15
to material...@googlegroups.com
Under QW 423.1, If he is qualified for P1, he gets qualified  up to P 15 F. 
You  have to keep 'F' nos  into consideration.

Sridhar
Mobile nos: 0 94449 71097,  0 94445 21267.


Please don't print this e-mail unless you really need to. Save the environment.




 


From: 'raouf salhi' via Materials & Welding <material...@googlegroups.com>
To: "material...@googlegroups.com" <material...@googlegroups.com>
Sent: Thursday, 22 October 2015 1:23 PM
Subject: Re: [MW:23773] Qualification of welders

Reply all
Reply to author
Forward
0 new messages