what are the effect of nitric acid and Sulphate in stainless steel pipe (material SS304)

36 views
Skip to first unread message

Shekh Sadik

unread,
Dec 22, 2024, 8:41:36 AM12/22/24
to Materials & Welding
Hello Experts,
Can anyone provide me some assistance regarding the subject.

Query:
what are the effect of nitric acid and Sulphate in stainless steel pipe (material SS304)

Details:
Sample contains 8.6 wt% of Sulphate. Total titratable acidity of the sample is 35.6 wt% as nitric acid.


vignesh Dhamoderan

unread,
Dec 23, 2024, 9:18:34 AM12/23/24
to material...@googlegroups.com
Hii,
Which standard cover interruption during pwht 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/7c23c7b7-c51d-4c4d-8cb0-843c644ea155n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages