Tanks PWHT

58 views
Skip to first unread message

Ahmed Sedeek

unread,
Jan 7, 2016, 9:31:26 PM1/7/16
to Materials & Welding
Dear Members,
 
We have crude and petroleum tanks in which 1 course of shell plates PWHT has to be carried out, so our subcontractor erect and install first , second and third course shell plate I asked if we could start welding in the second course and complete tanks shell without welding vertical and horizontal of the first course, and I want some document from code to approve this method if correct.
 
Regards,

Mohd Siraj

unread,
Feb 7, 2016, 3:57:42 AM2/7/16
to Materials & Welding
you are talking about the clean out door PWHT.

you can proceed the first ,second,third...with vertical joint first and horizontal after ward.

george keribo

unread,
Feb 9, 2016, 7:58:20 AM2/9/16
to material...@googlegroups.com
yes u can go ahead to weld the second course and the third courses
vertical joints since horizontal will be welded after the vertical has
been welded ...meaning the second and third course will be welded
before the horizontal connecting the first and second courses will be
welded...
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/703d865b-9790-4e1e-ba63-262b490692f2%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>