temper bead welding on S355JR hardened steel (Cold case)
21 views
Skip to first unread message
Nsizwa Nkosi
unread,
Feb 12, 2015, 10:26:05 AM2/12/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Aftternoon all
I am ivestigating the cause of cracking that occured on hardened S355 JR steel and if its possible to use temper bead on cold case. I would like to compile a welding repair procedure using temper bead welding on hardened S355 JR steel and would appreciate any suggestions and assinstance in the direction addresing this. I would also like to find out whether this practice will be possible or rather what can be suggested as an alternative.