Welding of nozzle made of AMS 5390 to C-276 pipe

30 views
Skip to first unread message

Ramesh Bapat

unread,
Dec 22, 2015, 10:37:18 PM12/22/15
to material...@googlegroups.com
Dear Experts
Can a nozzle made of AMS 5390 material be welded to C-276 pipe?
What process and what consumable and any precaution s Are these compatible
Kindly advise
Happy New Year
Ramesh

Sent from my iPhone

MW

unread,
Dec 23, 2015, 11:17:40 PM12/23/15
to Materials & Welding
In my opinion compatible would be ERNiCrMo-4  (UNS N10276) 