Dear Experts 


     We have wps it’s mentioned filler wire E71T-1CJ, but in the market available only E71T-1C. What is the difference between two filler wire and can we use E71T-1C instead of 1CJ

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

james gerald

unread,
Apr 21, 2024, 2:04:09 AM4/21/24
to material...@googlegroups.com
E71T-1C  is Charpy Impact tested at -20degC
E71T-1CJ is Charpy impact tested at -40degC.

AWS Classification for FCAW is only a supplementary requirement applicable only when Impact test is required.

If charpy impact test is not required then you can use E71T-1C in place of E71T-1CJ

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvvSvr_KHHb0thJJ2gotwiCMYU3TNsAwPcHgT_8f%2BDoLg%40mail.gmail.com.

saleem manhappulath

unread,
Apr 21, 2024, 2:39:42 AM4/21/24
to material...@googlegroups.com
Dear Sir

     Could you share, where it’s mentioned 


Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

Shahil Saini

unread,
Apr 21, 2024, 3:12:05 AM4/21/24
to material...@googlegroups.com
Dear saleem,

Please refer attached image,

Regards,
Shahil 

IMG_20240421_105229.jpg