Patch Plate Thickness - API 650 Tank

387 views
Skip to first unread message

shanmugam .N

unread,
Mar 2, 2020, 2:02:15 AM3/2/20
to material...@googlegroups.com
Dear Experts,

Construction Code: API 653
Annular PlateThickness: 13.5mm
Bottom plate thickness:8.0mm
       We are in a position to weld "Patch Plate" on the Annular ring plates.All the repairs are not in the critical zone (3"inch as per API 653). As per API 653 the patch plate thickness within the critical zone is  1/4" maximum. I could not get any reference for the patch plate thickness beyond the critical zone and within the annular ring plate.

Please kindly give your inputs with code reference.

With Regards,
N.S


shanmugam .N

unread,
Mar 3, 2020, 3:32:36 AM3/3/20
to material...@googlegroups.com
Dear Experts,

Construction Code: API 650
Annular PlateThickness: 13.5mm
Bottom plate thickness:8.0mm
       We are in a position to weld "Patch Plate" on the Annular ring plates.All the repairs are not in the critical zone (3"inch as per API 653). As per API 653 the patch plate thickness within the critical zone is  1/4" maximum. Could you please suggest the thickness requirement for the "Patch Plate" beyond the critical zone and within the annular ring plate.

Please kindly give your inputs with code reference.

With Regards,
N.S

With Regards,
N.Shanmugam


Kishor Swaminathan

unread,
Oct 11, 2020, 12:43:44 AM10/11/20
to material...@googlegroups.com

shanmugam


API 653 the patch plate thickness is same as the plate thickness

Regards,

KISHOR 
QC INSPECTOR 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaJw0%2Bfd%3Dc0uZ540d15RP80%2Bu3fRDDmiY5Vg9U3gY8e8zY7jA%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages