Cladded Material

51 views
Skip to first unread message

abdul sayeed mohammed

unread,
Nov 1, 2022, 5:17:07 AM11/1/22
to Materials-Welding
Dear Experts,
May you please give answers for the following photographs attached.
Thank you for your cooperation 
Best Regards 
Sayeed

Vishwas Keskar

unread,
Nov 1, 2022, 11:08:10 PM11/1/22
to material...@googlegroups.com
Query is not clear 
What CRA you want to do on Carbon steel?
What undiluted chemistry is specified and what depth ??
For PWHT  , what holding time temperature is envisaged ?
Pl specify the information . Then we can guide

Sent from my iPhone

On 01-Nov-2022, at 2:47 PM, abdul sayeed mohammed <mohammed.ab...@gmail.com> wrote:

Dear Experts,
May you please give answers for the following photographs attached.
71387c68-b8d7-46ca-969c-da3df9cd4e03.jpg
9e0094c0-7a1d-48dc-869c-6564600ef45f.jpg
f13edbd7-54ca-4793-858e-913a6f516cd2.jpg
Thank you for your cooperation 
Best Regards 
Sayeed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMH6-vx9JWL07o7DNuxDP2%3DbKR_eVuDyJbymvcYK737PL4W_-w%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages