72 views
Skip to first unread message

sujit kumar

unread,
Mar 2, 2023, 12:36:59 AM3/2/23
to material...@googlegroups.com
Dear all,

What filler wire we have to use to welding of SA516 GR.70 TO SB409UNSNO8810




Best Regards.
S.K

james gerald

unread,
Mar 2, 2023, 2:36:07 AM3/2/23
to material...@googlegroups.com
pls use ENiCrFe-3 and it also depends on the Design Temperature



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMxEnVrD2tCb4CXihObGTnhBLX02cFe8L0KQNePCCezMA%40mail.gmail.com.

sujit kumar

unread,
Mar 2, 2023, 5:55:10 AM3/2/23
to material...@googlegroups.com
Dear sir 
thank you for your reply....But  ENiCrFe-3  is the electrode but i want to know fiiler metal....Please reply.



Best Regards
S.k

james gerald

unread,
Mar 2, 2023, 6:21:46 AM3/2/23
to material...@googlegroups.com

Kannayeram Gnanapandithan

unread,
Mar 3, 2023, 12:08:15 AM3/3/23
to material...@googlegroups.com
u can use ERNiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


abdullah Alhiji

unread,
Mar 6, 2023, 7:47:33 AM3/6/23
to material...@googlegroups.com
Hi, the recommended filler metal for welding SA516 Gr.70 to SB409 UNS N08810 is a nickel-based alloy filler metal, such as Inconel 82 (AWS A5.14 ERNiCr-3) or Inconel 625 (AWS A5.14 ERNiCrMo-3). These filler metals are commonly used for welding dissimilar metals with high resistance to corrosion and high-temperature applications.

--