Can i know the general difference between ASME SEC IX and AWSD1.1 WPS/PQR.

Can i use ASME sec- IX WPS/PQR for any structural welding (Non-Impact). 
                 
              OR

Can i use AWS D1.1 WPS/PQR for any ASME related jobs (If qualified for butt weldings, Non Impact)


Please do needful.

--
Thanks and Regards, ?

Ghani,
Mechanical Inspector,



ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

mohd firdaus abd rahim

unread,
Nov 12, 2015, 4:08:30 AM11/12/15
to material...@googlegroups.com

Dear Mr Mohamed Ghani 

The requirement on ASME IX not same as AWS D1.1. The variable are the most clearly different in there. For example, ASME IX mention for joint configuration park on NON ESSENTIAL VARIABLE but on AWS D1.1 is contrary.

It depends on your client!

Few reputed clients accept ASME IX WPS in place of AWS D1.1.You can convinces your client by referring to API RP 582 - 2nd Edition, Clause 4.

Before approaching your client ,please ensure API RP 582 is applicable for the project.

 

4 General Welding Requirements

4.1 Structural (nonpressure boundary) welding requirements shall comply with either AWS D1.1 or AWS D1.6.

When approved by the purchaser (engineer) welding procedures may be qualified per ASME BPVC Section IX.”


Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjk35%3DUeKkOQS5Yy-npfk60e516PJB2qpVoh-GyoitNDg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages