Dear Experts,

Is there any tolerances for bottom plate distortions, as I checked only foundation tolerances are specified in API 650. As we have 45mm distortion observed in one of the plates, how can we control it, as per code.

sridhar cn

unread,
Apr 18, 2026, 8:47:34 AMApr 18
to material...@googlegroups.com

The observed distortion (~45 mm) exceeds acceptable industry practice and may lead to uneven stress distribution and 

loss of bearing. Typical industrial (not code mandated but widely accepted) practice is within 10 to 15 mm. 

As API 650 requires proper seating of bottom plates you can cut, refit, reweld to ensure  restoration of structural integrity 

and compliance with code requirements. 

Reduce the heat input by adopting sequence or skip welding methods and use strong back ups. Also check the foundation 

level before laying the plates. Use Laser level inplace of a straight edge. Trust it is clear.

Sridhar.

-----------------------------------------------------------------------------------------------------------------------------------------------------------------


On Sat, 18 Apr 2026 at 12:38, Raminshah Muhammed <ramin...@gmail.com> wrote:
Dear Experts,

Is there any tolerances for bottom plate distortions, as I checked only foundation tolerances are specified in API 650. As we have 45mm distortion observed in one of the plates, how can we control it, as per code.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/175e3d47-c294-4f11-a1f6-7ea014b68457n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages