Dear All,

Please comment on the weld metal properties of GMAW welded ASS with shielding gases 98%Ar+2%O2 and 98%Ar+2%CO2. How a shielding gas among these two will be selected.

Regards,
Sankalp

Mohd Siraj

unread,
Feb 5, 2022, 7:13:14 AM2/5/22
to Materials & Welding
depend on the mode of transfer,

for Gas details pl refer SFA 5.32 for details instead of random selection.

sridh...@yahoo.com

unread,
Feb 6, 2022, 7:01:22 AM2/6/22
to material...@googlegroups.com
Dear Mr. Sankalp,

As per AWS 5,32 following shielding gases are used for various metals.

AWS SG- AO -2       -----   98 Ar + 2 % O2 is used for SS 

AWS SG- A              ----- 100 Ar  for Aluminum  (or) 
AWS SG- He A-25   -----   75 He + 25 %  Argon  for Aluminum  (or) 
AWS SG- AHe-10    -----   90 Ar  + 10 %  Helium for Aluminum.

AWS SG-C               ----- 100 CO2  for Carbon Steel  (or) 
AWS SG- AC-20      -----   80 Ar + 20 % CO2 for Carbon Steel   (or) 
AWS SG- ACO -8/2 -----   90 Ar + 8 CO2 + 2 % O2 for Carbon Steel.

Other mixture gas ratios are also available for CS but, above are generally recommended.

C Sridhar.
-----------------------------------------------------------------------------------------------------------


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51256a9e-426b-4f23-8499-0685f046f412n%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Feb 7, 2022, 10:20:30 PM2/7/22
to materials-welding
o2 is better than co2 for ass, but either one can be used.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages