Position is not ess variable in wps


On Thu, 27 Jun 2024, 10:23 , <material...@googlegroups.com> wrote:
Chandrapal Singh <avio...@gmail.com>: Jun 26 10:10PM +0530

Is postion consider an essential variable in WPS.
If I have a WPS in 4G postion can i use that WPS in 1g, 2G, 3G position..
...more
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-weld...@googlegroups.com.

Nadakuditi kiran kumar

unread,
Jun 28, 2024, 7:47:20 AM (5 days ago) Jun 28
to material...@googlegroups.com
Dear Sir,

Which construction code you are following, for ASME Sec -IX, position not essential variable, but for AWS D1.1, it is essential.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGB1X9VCc0RrHhLKyvvm-GtH-7BKeTKacZ0c%3DHMqurot9XmD8Q%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages