Whom it may concern;
Has anyone had encountered STI welding?
Good Luck!
----- Original Message -----From: Fly YalungSent: Tuesday, June 10, 2008 8:30 AMSubject: [MW:837] Re: Thanx & STT welding procedure
surya prakash gajjall
ASSOCIATED ENGINEERING SERVICES
www.aesinspections.net.
We have shifted to E6010/GTAW root during the next phases of expansion
and STT machines were not used significantly.
STT is a good process provided your welding environment could be
controlled.
Regards,
P.M.Ganesan
Site QC Manager
QA&C Department
Kharafi National
P.O. Box: 24081, Safat - 13101, Kuwait
Mob: +965.7202358
Email: p.ga...@kharafinational.com
Website: www.kharafinational.com