The acceptability of performance qualification to other standards is the Engineer's responsibility, to be exercised based upon the specific structure, or service conditions, or both.

mbabu...@gmail.com

ungelesen,
17.01.2015, 12:00:5517.01.15
an material...@googlegroups.com
Dear,
Each standards have scope and limitations so we fallow the standard instructions.
Seniors better know.
Regards,
Babur khan Lashari
Sent from my BlackBerry 10 smartphone.
From: Raghuram Bathula
Sent: Saturday, 17 January 2015 18:23
To: Materials-Welding
Subject: Re: [MW:22729] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnvoFknLH9Jh%2B_igyfk5pUMjWZNhPi2ftvv6q803dpmOA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

pgoswami

ungelesen,
17.01.2015, 14:40:4417.01.15
an material...@googlegroups.com
Hi PKM,
 
Please see the appropriate clause as stated below.This is in line with the recommendations of Mr. Bhatula. Note the acceptance is not flat across the board, it's subject to engineer's discretion also.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 

4.2.2.1, Previous Performance Qualification. Previous performance qualification tests of welders, welding operators, and tack welders that are properly documented are acceptable with the approval of the Engineer. The acceptability of performance qualification to other standards is the Engineer's responsibility, to be exercised based upon the specific structure, or service conditions, or both.



From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of mbabu...@gmail.com
Sent: Saturday, January 17, 2015 10:29 AM
To: material...@googlegroups.com
Subject: Re: [MW:22730] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

Harikrishnan N S

ungelesen,
22.01.2015, 00:54:5922.01.15
an material...@googlegroups.com
Hi
 
Please refer the AWS D1.1 interpretation D1.1-08-I07 related to this subject.
 
 
Thanks and Regards
Harikrishnan

gprak...@gmail.com

ungelesen,
22.01.2015, 03:39:2822.01.15
an material...@googlegroups.com
Good info

Rgds
Prakash. G.
Independent Consultant. ASME/ISO/PED
From: Harikrishnan N S
Sent: Thursday, 22 January 2015 10:35
Subject: [MW:22742] Re: ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Allen antworten
Antwort an Autor
Weiterleiten
0 neue Nachrichten