I am having below clarification

What is the mechanical properties for below said grade material, which standard to refer
1.SAE 1018
2. ASTM A29, Grade:1018



Regards
Suresh

HENNING John

unread,
Mar 23, 2020, 11:07:27 PM3/23/20
to material...@googlegroups.com

1018 is an AISI designation that specifies chemistry only although standards other than the general ASTM/SA-A29 might specify.  AISI 1018 is a carbon steel with a nominal carbon content of 0.18%.

 

For example:

 

A/SA-311  Specification for cold-drawn, stress-relieved carbon steel bars subject to mechanical property requirements

 

Varies on diameter/thickness

Thickness/diameter

in. (mm)

Tensile

ksi (MPa)

Yield

ksi (MPa)

Elongation - RA

< 7/8 (20)

70  (480)

60  (415)

18 - 40

>7/8 (20) to < 1¼ (30)

65  (450)

55  (380)

16 - 40

>1¼ (30) to < 2 (50)

60  (415)

50  (345)

15 - 35

>2  (50) to < 3 (75)

55 (380)

45 (310)

15 - 35

 

 

 

 

 

You might also look at other specifications referenced in A/SA-29.

 

Hope this helps.  Code is fun.  “Live long and prosper” (Mr. Spock)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a7066f2f-0075-4d37-9c9c-f28526554fcc%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

José Juan Jiménez Alejandro

unread,
Mar 23, 2020, 11:07:28 PM3/23/20
to material...@googlegroups.com
Check the Reference Code (SAE or ASTM) or the specification of the material, in those documents the properties come to details, but that is a research work that corresponds to you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a7066f2f-0075-4d37-9c9c-f28526554fcc%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





SURESH

unread,
Mar 24, 2020, 12:33:31 AM3/24/20
to Materials & Welding
Thank you very much for the information shared

To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Reply all
Reply to author
Forward
0 new messages