With regards to Long seam you will get from ASME Sec VIII UW-9, But silent for Circ Seam However, Good Engineering Practices and One of client specification
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAM%2ByfweOirWgGkCu322YeeSmv8SVb_dbp5jsTJaEt7LR4p7Dtg%40mail.gmail.com.
Client specification Min. 50 mm Distance have to be maintained
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/419a169f-f63b-4015-8f8a-004c86e35671n%40googlegroups.com.
CONFIDENTIALITY NOTICE: This communication, and the information it contains, is (a) intended for the person(s) and/or organisation(s) to whom it is addressed and is for no other person(s) or organisation(s) and (b) may be confidential, legally privileged and protected by law, including law of copyright. Unauthorised use, copying, forwarding or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by telephone to our head office number. We process personal data for the purposes explained in our privacy notice, which can be found here: https://www.dornan.ie/ privacy-policy/ . This notice also contains information about your rights.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGFjgNH1xcokLxoXXc2kA9ngfL0wwEVEPJE8UVSj8SUboKrQyw%40mail.gmail.com.