Heat treatment cycle preparation

107 views
Skip to first unread message

Shahil Saini

unread,
Jan 4, 2022, 10:15:14 PM1/4/22
to material...@googlegroups.com
Hello everyone,
using ASME B31P Standard Heat Treatment for Fabrication Process, How i prepare my heat treatment cycle? Table 6.1.1-1 is showing soaking temperature and time, where i can find loading, unloading temperature, rate of heating and cooling?, and how i decide how many cycle is required?

Regards,
Shahil Saini,
PGET- Welding Engineer

SN

unread,
Jan 6, 2022, 4:10:41 AM1/6/22
to material...@googlegroups.com
Dear all,

Can we requalify  welding consumables (electrode and wires) once the shelf life is over.

As ASME code gives any guideline to requalify  the welding consumables.

Kindly provide your expert opinion on this.

Vishwas Keskar

unread,
Jan 6, 2022, 10:11:03 PM1/6/22
to material...@googlegroups.com
Pl specify clear context of Requalification of consumables. 
Let us understand what you mean
Thanks 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.

Syed Gohar Abbas Zaidi

unread,
Jan 7, 2022, 3:08:44 AM1/7/22
to material...@googlegroups.com
Dear,

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


--



Regard's:

Syed Gohar Abbas Zaidi
Cell No.: 0092-324-1407544

MW

unread,
Jan 7, 2022, 3:13:47 AM1/7/22
to Materials & Welding
pl. refer old posts in the group
Screenshot 2022-01-07 134237.jpg

james gerald

unread,
Jan 7, 2022, 5:04:44 AM1/7/22
to material...@googlegroups.com
Normally we do not use welding consumables beyond the Shelf life as recommended by welding consumable manufacturer. I have physically seen Flux coating peeling off from the electrode. It is better to contact the welding consumable manufacturer and if they recommend better to do consumable testing as per ASME Sec.IIC at the manufacturer's premises.

Thanks & Regards

J.Gerald Jayakumar




pgos...@rogers.com

unread,
Jan 7, 2022, 9:48:39 AM1/7/22
to material...@googlegroups.com

Hi ,

Every welding consumable has a “shelf life”. Please see the guidance from ESAB on typical shelf life of various SMAW electrodes & other FCAW products. Shelf life matters a lot , on how the consumables are manufactured and subsequently stored.

Sec-IX , would not provide any guidance on welding consumables.

If needed all weld metal testing may be performed as per ASME Sec-II, Part C.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

IndependentWelding & Metallurgical Engineering Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of MW
Sent: January 7, 2022 3:14 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: Re: [MW:32736] Requalification of consumable after shelf life

 

pl. refer old posts in the group

 

On Friday, 7 January 2022 at 13:38:44 UTC+5:30 Syed Gohar Abbas Zaidi wrote:

Dear,

 

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

 

On Thu, Jan 6, 2022 at 12:10 PM SN <suryawans...@gmail.com> wrote:

Dear all,

 

Can we requalify welding consumables (electrode and wires) once the shelf life is over?

 

As ASME code gives any guideline to requalify the welding consumables.

 

Kindly provide your expert opinion on this.

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


 

--

 

 

 

Regard's:

 

Syed Gohar Abbas Zaidi

Cell No.: 0092-324-1407544

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


image001.jpg
gen-27116_shelf_life_storage_reconditioning_of_filler_metals.pdf

james gerald

unread,
Jan 9, 2022, 10:17:31 PM1/9/22
to 'james gerald' via Materials & Welding
Just for info.

That is why Inventory control is very critical in Fabrication industry. You need to estimate the correct quantity and procure them. Moreover you quantify the welding consumable as stock items and critical items. Special consumable come under critical items and normal moving used items like carbon steel come under stock items.

If consumable after shelf life is small quantity then you can use it for welder training purpose else if it is a Large quantity then better to contact welding consumable manufacturer.

Thanks & Regards

J.Gerald Jayakumar


Vinay Thattey

unread,
Jan 9, 2022, 10:17:42 PM1/9/22
to material...@googlegroups.com, suryawans...@gmail.com

pl elaborate. 

In general electrodes have an expiry date of about 24 months from date of manufacturing .. In my view it has to be disposed of . 

Manufacturer specifies the minimum warranted life of flux cored electrodes. 

The issue is shelf life is in general not mentioned on product description /certificates of rod/wires e.g.  19Cr/12Ni/Mo type solid wire for MIG .

I have not seen any guidance or recommendation of code/standard on your query ..


--

Kannayeram Gnanapandithan

unread,
Jan 18, 2022, 12:11:42 AM1/18/22
to materials-welding
No welding consumable manufacturers are recommending self life of consumables. 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349