410 WPS PQR

69 views
Skip to first unread message

Vishwas Keskar Welding Manager WELDING

unread,
Nov 15, 2022, 3:51:41 AM11/15/22
to Materials & Welding
Experts,

Pl. guide for qualifying PQR for SA 240 TYP 410 without PWHT .
Pl, guide for Pre heating, inter pass  temperature, consumable to be used 
Thickness of job is 8 mm , 10mm

Thanks and regards
Vishwas - IWE
International Welding Engineer 
Head - Welding Technology

 

Ahmed Osman

unread,
Nov 15, 2022, 5:09:46 AM11/15/22
to Materials & Welding
if BM carbon <= 0.08% .. u can do it without PWHT .. E309L-16 .. preheat 300c and interpass < 300C 
else PWHT is essential for avoiding cracks 
U can go for 410S if possible

Best Regards ,
Ahmed Osman

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8369c986-7b85-44d3-b06c-2670d887ee26n%40googlegroups.com.

chandraknat vaidya

unread,
Nov 27, 2022, 10:27:00 PM11/27/22
to material...@googlegroups.com
Use of 309L weldmetal is appropriate.

--

Vishwas Keskar

unread,
Nov 28, 2022, 2:35:48 AM11/28/22
to material...@googlegroups.com
Yes 
Will use based on service conditions
Thanks 

Sent from my iPhone

On 28-Nov-2022, at 8:56 AM, chandraknat vaidya <vaid...@gmail.com> wrote:



Kannayeram Gnanapandithan

unread,
Nov 28, 2022, 10:14:42 PM11/28/22
to materials-welding