welder certification

20 views
Skip to first unread message

Rilley Chellah Mulenga

unread,
Nov 6, 2025, 10:47:56 AMNov 6
to material...@googlegroups.com
Good day technical experts,

Can I use a WPS for S355jr thickness of 30mm plate in SMAW to qualify a pipe S355jr 6mm thick in SMAW ? your quick response is highly appreciated  

--
RILLEY CHELLAH MULENGA
Materials Evaluation Head of Department
E: rilley....@ahkgroup.com
CompanyLogo
 


DISCLAIMER: The information in this Internet e-mail is confidential and may be legally privileged. It is intended solely for the addressee(s).
Access to this Internet e-mail by anyone else is unauthorised.

If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is prohibited and may be unlawful.
All results and data contained in this document are subject to our Standard Terms and Conditions and are valid only when supported by an original document.

Please visit our website at www.ahkgroup.com

venkateswara reddy Desireddy

unread,
Nov 6, 2025, 10:00:02 PMNov 6
to material...@googlegroups.com
In WPS document qualified material thickness range and P number range available, 
Based on that you can select the WPS.
As per ASME Sec IX you can use plate WPS for pipe. But must be required same P number.
Before using WPS you have to conform all essential variables.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHkXHT84wQHJDjOio6eAbwpnQX6Zu29uhEkGAtv-jXvEPCTArA%40mail.gmail.com.

Bala Murugan

unread,
Nov 6, 2025, 10:00:03 PMNov 6
to material...@googlegroups.com
Heloo Mr Rilley,
I hope your WPS qualifies as per ISO 15614-1 . Can you clarify if your category is Level1 or Level 2? What about Pipe OD?

No, as per ISO 15614-1, a Welding Procedure Specification (WPS) qualified on S355jr plate with 30mm thickness using SMAW does not qualify you to weld S355jr pipe with 6mm thickness using the same WPS. The essential thickness qualification range for butt welds is based on the thickness of the test piece and differs for plate and pipe, especially when moving from plate to significantly thinner pipe.

Plate-to-Pipe Qualification Limits

  • Plate test pieces generally only qualify pipe if the pipe’s outside diameter is greater than 500mm, or if the diameter is more than 150mm and welded in the PA or PC (rotated) position. For smaller pipe diameters or significantly lower wall thickness, separate qualification is required.

  • In your specific case (30mm plate → 6mm pipe SMAW, S355jr), you cannot directly use the WPS without further qualification of the pipe if the diameter limitations above are not met.


 Pls find the attached Code extract for your reference.
image.png
image.png
Thanks & Regards,
Balamurugan

--

Rilley Chellah Mulenga

unread,
Nov 7, 2025, 4:36:42 AMNov 7
to material...@googlegroups.com
Good day Bala,

We are using ASME IX other than ISO 15616-1

Rilley Chellah Mulenga

unread,
Nov 7, 2025, 4:36:42 AMNov 7
to material...@googlegroups.com
Goodday  venkateswara ,

The thickness range qualified in the WPS according to ASME IX is 1.5 to 30mm and the P no is 1 because the material is the same S355JR steel 


Bala Murugan

unread,
Nov 7, 2025, 7:26:44 AMNov 7
to materials-welding
As per Asme section 9, yes you can use that WPS if all the essential variables like p no, f no matches ....you can use that WPS 