Dear Experts,
 
As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------

 Wps approved for groove joint is applicable for fillet joint?

  If so where it is stated.

cordially,
Jay Poojary

Jim Price

unread,
Sep 29, 2015, 7:52:20 AM9/29/15
to material...@googlegroups.com

ASME Section IX QW303.2 and QW461.9 gives you the positions qualified for

 

Best Regards

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimp...@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySZQkp22fraccZK2Eohv1k-CisD_Z2_p7XssaRAf9YEaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

p_cha...@mail.bg

unread,
Sep 30, 2015, 12:09:32 AM9/30/15
to material...@googlegroups.com

Dear Mr. Poojary,

QW-202.2(c) says:
''Qualification for Fillet Welds. WPS qualification for fillet welds may be made on groove-weld test coupons using test specimens specified in (a) or (b). Fillet-weld procedures so qualified may be used for welding all thicknesses of base metal for all sizes of fillet welds, and all diameters of pipe or tube in accordance with Table QW-451.4. Nonpressure-retaining fillet welds, as defined in other Seetions of the Code, may as an alternate be qualified with fillet welds only. Tests shall be made in accordance
with QW-180. Limits of qualification shall be in accordance witb Table QW-451.3.''

Table QW-451.4 Fillet Welds Qualified by Groove-Weld Tests shall also be considered.

Best regards

Parvan Chavdarov

Dr.-Ing. Parvan Chavdarov
ASME A, B & N Inspector,IWE
Business Unit Nuclear Safety

TÜV Rheinland Industrie Service GmbH
Am GrauenStein
51105 Köln
Tel.: + 49 221 806 4251
Fax: + 49 221 806-3402
Mobile: + 49 151 53171362
parvan.c...@de.tuv.com

----- Цитат от Jay Poojary (jayo...@gmail.com), на 28.09.2015 в 17:18 -----

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySZQkp22fraccZK2Eohv1k-CisD_Z2_p7XssaRAf9YEaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



Dr.-Ing. Parvan Chavdarov



ASME A, B & N Inspector, IWE



Business Unit Nuclear Safety



 



TÜV Rheinland Industrie Service GmbH



Am Grauen Stein



51105 Köln



Tel.: + 49 221 806 4251



Fax: + 49 221 806-3402



Mobile: + 49 151 53171362



parvan.c...@de.tuv.com



-------------------------------------
Mail.BG: Безплатен e-mail адрес. Най-добрите характеристики на българския пазар - 20 GB пощенска кутия, 1 GB прикрепен файл, безплатен POP3, мобилна версия, SMS известяване и други.

Reply all
Reply to author
Forward
0 new messages