Next edition of Section IX will have rules for fusion of HDPE.


-----Original Message-----
From: material...@googlegroups.com on behalf of Thandion
Sent: Sat 5/18/2013 3:26 AM
To: material...@googlegroups.com
Subject: [MW:17697] Welder Qualification with HDPE electro fusion weld

Good afternoon gents,

I have a question regarding welder qualification (performance records)
procedures for HDPE pipe electrofusion butt weld. I couldnt find any
reference in ASME standards for;

- Qualification diameter, thickness range
- Qualified materials
- Which destructive tests should I send frist production material

Which standard reference should I follow? (ASTM D3261 maybe?)


Ps. Welders already have certificate that required by the country I am in.
All I need is to test them like we do in steel piping.


Thanks&Regards,
Tarik

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
winmail.dat

Naveen Raj

unread,
Jan 13, 2017, 2:39:00 AM1/13/17
to Materials & Welding
Hi,

You should check EN 13067 - Plastics welding personnel. Qualification testing of welders. Thermoplastics welded assemblies for welder qualification of EF welders.