Dear all
Please clarify below
1 . Minimum deposit weld metal thickness 2 mm acceptable as per ASME sec IX &API 6A corrosion resistance overlay
2 . Please refer the attached photos for macro examination fusion line waveform acceptable or not for overlay please guide me
Regards
ELAVARASAN