Acceptance criteria for distortion

492 views
Skip to first unread message

Samiulla Syed

unread,
Oct 1, 2021, 4:36:37 AM10/1/21
to material...@googlegroups.com
Dear Expert

Can some help to get the distortion acceptance criteria to WQT at 4G position.

--

--
Best Regards
Samiulla Syed,
Senior Trainer,
Welding Department,
TUV Rheinland Arabia LLC
National Industrial Training Institute,
Al Ahsa,
Eastern Province,
Kingdom of Saudi Arabia,
Email: ss...@niti.edu.sa
          qcsye...@gmail.com
Mobile: +966(0)595531593.

james gerald

unread,
Oct 4, 2021, 2:37:14 AM10/4/21
to material...@googlegroups.com
The distortion may be due  to lack of sufficient Stiffeners and supports.

Normally the Type of Distortion which occurs is as below.


Inline image



There are no specific requirements to Distortion while qualifying the WQT. Even WQT's of pipes are being successfully Radiographed. Hence as long as you are able to Radiograph 6inch (150mm) successfully, WQT is considered acceptable.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFRNJK8xjqNeVZqH8mPSiJXiGOeyRarkk%3Dj3qytygKrBKVVRMA%40mail.gmail.com.

james gerald

unread,
Oct 4, 2021, 4:25:56 AM10/4/21
to 'james gerald' via Materials & Welding
Just to add,

if Distortion is being observed during WQT welding which results in Closing or opening up of Weld Bevel then normally TPI's do not permit Grinding to set right the bevel and in this case a new WQT required to be Qualified.

Nornally by using strong supports(Stiffeners) and proper Tacks or Bridge Tacks the bevel during WQT qualification can be protected.

Thanks & Regards

J.Gerald Jayakumar