Dear Experts,

 

Can  you recommend the filler in ER series  for welding  Monel 400  to  Carbon Steel (A105)  material.

 

Thanks and regards

S G Dixit

Sr. Manager- Materials

vaibhav Joshi

unread,
Mar 22, 2012, 1:24:02 AM3/22/12
to material...@googlegroups.com
Dear

ErNiCu1 or ERNiCu7 both are compitible. Preheat CS to atleast 75 deg c to avoid any cracking.


VJ

On Thu, Mar 22, 2012 at 10:57 PM, Dsunil <dsu...@gicongoa.com> wrote:

Dear Experts,

 

Can  you recommend thet filler in ER series  for welding  Monel 400  to  Carbon Steel (A105)  material.

 

Thanks and regards

S G Dixit

Sr. Manager- Materials

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Prakash Hegde

unread,
Mar 23, 2012, 7:17:04 AM3/23/12
to material...@googlegroups.com
Hi!
Best filler is ER NiCu7 for monel to monel and discimilar metal welding
Regards
Hegde P.B.