Minimum distance between two circumferential pipe joints

79 views
Skip to first unread message

port dickson

unread,
May 22, 2023, 3:49:50 AM5/22/23
to Materials & Welding
Dear Experts,

                              We need your advice regarding minimum distance requirements between 2 circumferential pipe joints .

SENTHIL P

unread,
May 22, 2023, 4:43:34 AM5/22/23
to MATERIAL
Mini 4t,t -thickness of pipe

On Mon, 22 May, 2023, 3:49 PM port dickson, <gokulgo...@gmail.com> wrote:
Dear Experts,

                              We need your advice regarding minimum distance requirements between 2 circumferential pipe joints .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7f549eff-946d-485e-9f5a-4ee1fd56890dn%40googlegroups.com.

Parminder Singh

unread,
May 22, 2023, 4:52:04 AM5/22/23
to Materials & Welding
minimum 4t 

Srinivas Rao

unread,
May 22, 2023, 6:18:25 AM5/22/23
to Materials & Welding
Check consruction code and client specification for minimum diatances between welds , each will have a different recommentdations . refer and follow 
Example : ASME B 31.3 - does not given any recommendations on this subject.

Regards,
Srinivas Rao
Welding Engineer 

Alcindo Jardim

unread,
May 22, 2023, 7:40:31 AM5/22/23
to material...@googlegroups.com
Please see the attached file
Alcindo O. J. Jr.
21 96676-1511



Em seg., 22 de mai. de 2023 às 04:49, port dickson <gokulgo...@gmail.com> escreveu:
Dear Experts,

                              We need your advice regarding minimum distance requirements between 2 circumferential pipe joints .

--