HOW TO REBUILD A WORN-OUT WIRE DRAWING DRUM BY WELDING

25 views
Skip to first unread message

Adil c

unread,
Jan 1, 2017, 10:01:33 PM1/1/17
to Materials & Welding
Hi Experts,

I need your suggestions on rebuilding of a wire drawing drum by welding. (Please find the attached photographs)

1. I need to know what could be the exact base material used for the normal wire drawing drum. (Please find the attached photographs)
2. What is the optimum hardness recommended to withstand high wear resistance of longer wire drawing.
3. Which alloy combination is recommended for the welding electrode that needs to be used.
4. Should i use any low heat input electrode, hardfacing electrode or conventional electrodes with high tensile properties(E12018 - G)...etc.



Regards

Adil. C
IMG_2021.JPG
IMG_2022.JPG
IMG_2024.JPG
IMG_2079.JPG