So the samples we sent all used 60um NiAl nanofoil
#1 in the center of the gel-pack was a Cu shim and assembled on the Al jig.
#2 in the lower left was a Mo shim assembled on the Teflon jig
#3 in the lower right was a Cu shim assembled on the Teflon jig