海妹,小乖, 小赖指点一下?

 

From: z0912021@google


     
有朋友生产汽车内饰件,对于工艺寻求帮助\指教。问题是怎样解决加工过程中的烟雾过大问题。
     
流层是木粉+PP颗粒+PP回首物,然后加温压缩成型,出料时烟雾过大。PP颗粒160度熔解,机器加温时温度在400度。

Zhu, Charlie

unread,
Nov 8, 2011, 10:34:30 PM11/8/11
to f010...@googlegroups.com

真空。。。

 

Thanks,

Best Regards,

Charlie Zhu (ZHU LI)


--
F0106102班级邮箱: F010...@googlegroups.com
F0106102班级论坛: http://groups.google.com/group/F0106102?hl=zh-CN
I'll be there for you, 'cause you're there for me too!

刘学海

unread,
Nov 9, 2011, 2:55:26 AM11/9/11
to f010...@googlegroups.com
生产PP木粉板的?找设备供应商支持一下:D Sent from my Motorola phone.

Li, Daniel UTCFS

unread,
Nov 9, 2011, 8:57:26 PM11/9/11
to f010...@googlegroups.com

我这里显示都是乱码

 

From: f010...@googlegroups.com [mailto:f010...@googlegroups.com] On Behalf Of 刘学海
Sent: 2011
119 15:55
To: f010...@googlegroups.com
Subject: Re: [F0106102] FW:
汽车内饰件工艺求助

 

ɺPPľ۰ՒɨӦɌ֧֒ς:D Sent from my Motorola phone.



"Li, Daniel UTCFS" <Dani...@fs.utc.com> wrote:

Ã,СԼ/span>, С5ָς?

 

From: z0912021@google


      ӐųӑɺƻĚʎ,ԓڹҕѰdz\ָ̡Ί̢ʇԵѹ⾶ӹ̖еđ̎?󎊌
      w㊇ľۼspan lang=EN-US>+PPŁ+PP؊׎Ȼ󼓎‘˵ɐͣ??ьέ󡣼span lang=EN-US>PPŁ160Ȉ۽ƷӎŠ΂Ȕڼspan lang=EN-US>400ȡ

--
F0106102
ӊϤ: F010...@googlegroups.com
F0106102
̳: http://groups.google.com/group/F0106102?hl=zh-CN


I'll be there for you, 'cause you're there for me too!

Li, Daniel UTCFS

unread,
Nov 9, 2011, 8:59:21 PM11/9/11
to f010...@googlegroups.com

设备完全不一样了, 从现有工艺上有没有改进的空间

 

From: f010...@googlegroups.com [mailto:f010...@googlegroups.com] On Behalf Of Zhu, Charlie
Sent: 2011
119 11:35
To: f010...@googlegroups.com
Subject: [F0106102] RE:
汽车内饰件工艺求助

 

真空。。。

 

Thanks,

Best Regards,

Charlie Zhu (ZHU LI)


From: f010...@googlegroups.com [mailto:f010...@googlegroups.com] On Behalf Of Li, Daniel UTCFS
Sent: Wednesday, November 09, 2011 10:14 AM
To: f010...@googlegroups.com
Subject: [F0106102] FW:
汽车内饰件工艺求助

 

海妹,小乖, 小赖指点一下?

 

From: z0912021@google


     
有朋友生产汽车内饰件,对于工艺寻求帮助\指教。问题是怎样解决加工过程中的烟雾过大问题。
     
流层是木粉+PP颗粒+PP回首物,然后加温压缩成型,出料时烟雾过大。PP颗粒160度熔解,机器加温时温度在400度。


I'll be there for you, 'cause you're there for me too!

Reply all
Reply to author
Forward
0 new messages