Hi everyone,
I hope you're doing well.
I am currently working on creating a laminated glass configuration:
9/16" Laminated Glass – 1/4" HS Low Iron + 0.09 PVB + 1/4" HS Low Iron. see attachment
However, I could not find this specific configuration in Windows. As a result, I created it in Optics, but I encountered an issue—Optics flipped the layers. It seems that Optics does not allow the Low-E coating to be in direct contact with the interlayers.
Would you happen to know a solution for this? Any guidance on how to properly configure this glass in Optics while maintaining the correct layer order would be greatly appreciated.
Please let me know your thoughts. Thank you in advance for your help!
Best regards,--
You can view the THERM forum online at:
https://groups.google.com/g/LBNL-THERM
---
You received this message because you are subscribed to the Google Groups "THERM" group.
To unsubscribe from this group and stop receiving emails from it, send an email to LBNL-THERM+...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/LBNL-THERM/ac58106e-8247-423e-a4be-68e768047d0an%40googlegroups.com.