| Dear All, In some of the materials we need to go for 0.2% offset method for Y.S. Why? & 0.2% of which value is to be calculated? Thanx & Regds, PSP |
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| Percent elongation = 100 |
|
| Percent reduction in area = 100 |
|
Dear Prashantpan:
In some materials, the stress at which the material changes from elastic to plastic behavior is not easily detected.
In this case, the offset yield strength is determined. A line is constructed parallel to the initial portion of the stress-strain curve but offset by 0.002 in/in (0.2%) from the origin.
The 0.2% offset yield strength is the stress at which the constructed line intersects the stress-strain curve as shown:

| Dear Sir, Can u give one example for the same? Thanx & Regds, PSP --- On Wed, 3/8/11, Ramin Kondori <ramink...@gmail.com> wrote: |
| Dear All, In some of the materials we need to go for 0.2% offset method for Y.S. Why? & 0.2% of which value is to be calculated? Thanx & Regds, PSP |