Dear all,

What difference "welder" and "welding operator" stated in ASME IX?

Karthik

unread,
Aug 18, 2010, 3:48:47 AM8/18/10
to material...@googlegroups.com

Hi,

Please find below the definition of welder and welding operator and tack welder.

WELDER:

A welder is one who performs a manual or semiautomatic welding operation.This includes welding with torch,gun or electrode holder held and manipulated by hand.Part motion devices and manually controlled filler metal feeders may be used.Semi automatic welding is manual welding with equipment that automatically controls one or more of the welding conditions,usually filler wire feed.A welder would commonly perform shielded metal arc,gas metal arc,and flux cored arc welding.


WELDING OPERATOR:

A welding operator is one who operates adaptive control,automatic,mechanized,or robotic welding equipment.Automatic welding is with equipment that reqires occasional or no observation of the welding and no manual adjustments of the welding controls.Mechanized welding is with equipment that requires manual adjustment of the equipment controls in response to visual observation of the welding,with torch,gun or electrode holder held by a mechanical device.Most submerged arc welding setups would fit in to this category.


TACK WELDER:

A tack welder is a fitter,or someone under the direction of a fitter,who tack welds parts of a weldment to hold them in proper alignment until the final welds are made.


Thanks & Regards,


(Karthik)


Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 8/18/10, skrie85 <skr...@yahoo.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

MNS

unread,
Aug 18, 2010, 5:36:33 AM8/18/10
to Materials & Welding
Simple Definition given ASME Sec IX

1) Welder: one who performs manual or semiautomatic
welding.

2) Welding Operator: one who operates machine or automatic
welding equipment.

skrie85

unread,
Aug 18, 2010, 4:58:54 AM8/18/10
to material...@googlegroups.com
Tack welder need to qualify or not?


From: Karthik <karth...@yahoo.com>
To: material...@googlegroups.com
Sent: Wed, August 18, 2010 3:48:47 PM
Subject: Re: [MW:6556] Difference welder and welding operator

Sakib

unread,
Aug 18, 2010, 3:09:58 AM8/18/10
to material...@googlegroups.com

word operator is used for Automatic machines such as SAW




--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556

mayur purwant

unread,
Aug 18, 2010, 9:53:02 AM8/18/10
to material...@googlegroups.com
You have to qualify tack welders, because finally you r going to put them on job.
 
Regards,
 
Mayur Purwant
Welding
Godrej & Boyce

Potter, Richard

unread,
Aug 18, 2010, 11:51:51 AM8/18/10
to material...@googlegroups.com

When tack welds remain as part of the final weld they must be applied by a qualified welder.

Thus, you will have to qualify tackers in accordance to ASME Section VIII Div.1 UW-31 Paragraph 3

 


Kathalingam Babu

unread,
Aug 18, 2010, 8:48:27 PM8/18/10
to material...@googlegroups.com
Hi
 
As per AWS D1.1 , Tack welder have  to qualified.
 
As per ASME Sec IX , tack welder has to be qualified by fillet weld qualification.
 
Rgds,
 
K.Babu
Singapore