Dear all,

  Could you please inform where's mention the visual welds examination acceptance criteria on ASME sect I.

Thank you.

--

Thanks and Regards, 

dilintas

unread,
Mar 28, 2017, 10:14:59 AM3/28/17
to material...@googlegroups.com
Are stated in the part PWHT of section I



Sent from my Samsung Galaxy smartphone.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB2cMm8b1eAYNbu2KGv-n7VT2twKTDw-rFNCypdF39S5%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
Mar 28, 2017, 10:43:37 AM3/28/17
to materials-welding
PW35

On 28-Mar-2017 7:44 PM, "dilintas" <dili...@gmail.com> wrote:
Are stated in the part PWHT of section I



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Zakaria ghrab <zakari...@gmail.com>
Date: 27/03/2017 19:07 (GMT+02:00)
Subject: [MW:26291] ASME sect I, Visual welds examination acceptance

Dear all,

  Could you please inform where's mention the visual welds examination acceptance criteria on ASME sect I.

Thank you.

--

Thanks and Regards, 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/yvr5xfde933gphaj0r8nxmka.1490634686353%40email.android.com.
Reply all
Reply to author
Forward
0 new messages