to material...@googlegroups.com

Dear exparts,
 
Can any one guide me about welding simulator ..what's advantage & disadvantages

Regards

Sudip

*** This message has been sent using GIONEE M3 ***

Alan Denney

unread,
Sep 29, 2015, 3:41:40 AM9/29/15
to material...@googlegroups.com

The Gleeble welding simulator can subject a small sample of steel to a similar thermal cycle to that experienced by some part of the steel during welding, thus creating, in the whole width of the specimen the metallurgical structures which would normally exist only in a very narrow band or local area of the heat affected zone of the weld. This can then be used as a means of studying the properties and structure of these discrete microstructures. The thermal cycle has to be programmed into the machine from prior investigations.

 

The disadvantage is, I suspect, that HAZs contain areas of poor properties which are constrained by the surrounding material and if you test the HAZ of an actual weld these areas do not dominate the overall properties. In the simulated specimen you have a lot more of that microstructure and you will discover the true base values of toughness, for example.

 

A Google search on the term Gleeble should give you  a lot more information.

 

Alan Denney

AKD Materials Consulting Ltd

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/u40bjjxdkxm8l81ai051gu55.1443503441312%40email.android.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
Reply all
Reply to author
Forward
0 new messages