Dear Experts,
Crack observed in Base material- IS 10748 gr 2 to EN45A(Tempered ).
Base material thickness-4 mm
Fillet size-4 mm
Welding process-GMAW
Filler Wire-ER70S6.

Experts need your valuable suggestions.