No, in most of the cases.
32750 is a SDSS(25Cr), while 31803 is a DSS(22Cr). For P10H group every grade is different, in chemistry, mechanical properties & corrosion resistance. You require separate PQR with all comprehensive testing for each individual grade.
What’re the process requirements and intended service/s.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent Welding & Metallurgical Engineering Specialist
Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)
Saudi Aramco Approved Designated Project Welding Engineer (DPWR)
Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
Thanks & Regards
J.Gerald Jayakumar