Please refer BSEN 10204 for.more information
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Hi
Based on the criticality rating of the equipment's, the material certification requirements are decided.
Refer the pump MR (Maternal Specification), project purchase material specification / pump data sheet, there you can get the complete information.
Regards
P Govindan
Hi
2.2 certification is a certificate contains compliance of a product (COC) or un tested data of a product.
3.1 certification is a certificate contains the physical and chemical properties / performance tests are tested at manufacturer laboratory or outside accredited laboratory and the tests are witnessed by the quality department of the manufacturer. Simple we can call as a manufacturer quality certificate.
3.2 certificate is a certificate contains all the physical & chemical properties / all the performance tests/FAT (Factory Acceptance Tests) are witnessed by both quality department personnel of the manufacturer and third party inspection agency's Inspector.
I hope above information clear about the certification levels.
Regards
P Govindan
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f794a65b-0632-4fe1-b9e0-7ed4a33c9c5an%40googlegroups.com.